Journal article
Fracture toughness of seven resin composites evaluated by three methods of mode I fracture toughness (KIc)
A Mese, JEA Palamara, R Bagheri, M Fani, MF Burrow
Dental Materials Journal | JAPANESE SOC DENTAL MATERIALS DEVICES | Published : 2016
DOI: 10.4012/dmj.2016-140
Abstract
This study compared the fracture toughness values of seven resin composites and analyzed the consistency of data values using three methods: compact tension, three point and four point bending for Mode I failure. Seven resin composites were selected: Estellite Sigma Quick, Esthet X HD, Filtek Supreme XTE, Heliomolar, Ice, Rok, and Vit-l-escence. For each material, 18 specimens (n=6 for each test) were prepared. Maximum load to failure was recorded using a universal testing machine and fracture toughness was calculated. There was a direct significant correlation among all tested methods. Rok showed the highest and Estelite the lowest KIc values. SEM of the fractured surface of compact tension..
View full abstract